tensile fatigue-creep testing: A powerful tool to simulate
Journal of power sources ; 312
2016
Article (Journal)
English
Tensile creep behavior and cyclic fatigue/creep interaction of hot-isostatically pressed SiN
Automotive engineering | 1991
|Creep in high temperature tensile testing of rhenium
AIAA | 2000
|Automotive engineering | 2011
|British Library Conference Proceedings | 2011
|