Fatigue-crack-propagation and fracture-toughness characteristics of 7079 aluminum-alloy sheets and plates in three aged conditions
NASA contractor report ; CR-996
1968
V, 93 S
Ill., graph. Darst
Contract no.: NAS 1-6474
Report
English
ALUMINUM ALLOY EXTRUSIONS 4.3Zn - 3.3Mg - 0.60Cu - 0.20Mn - 0.18Cr (7079-T6)
SAE Technical Papers | 1981
Aluminum Alloy Forgings, 4.3Zn - 3.3Mg - 0.60Cu - 0.20Mn - 0.18Cr (7079-T6)
SAE Technical Papers | 2006
ALUMINUM ALLOY EXTRUSIONS 4.3Zn - 3.3Mg - 0.6Cu - 0.2Mn - 0.17Cr (7079-T6)
SAE Technical Papers | 1960
ALUMINUM ALLOY FORGINGS 4.3Zn - 3.3Mg - 0.60Cu - 0.20Mn - 0.18Cr (7079-T6)
SAE Technical Papers | 1995
ALUMINUM ALLOY FORGINGS 4.3Zn - 3.3Mg - 0.6Cu - 0.2Mn - 0.2Cr (7079-T6)
SAE Technical Papers | 1955