Steel, Corrosion-Resistant, Investment Casings 15Cr - 4.0Ni - 2.3Mo - 0.09N Solution Heat Treated
Titanium Alloy, Round Bars 5Al - 1Fe Annealed
Equivalent Sections of Certain Shapes to Round Bars
Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
Steel, Mechanical Tubing 0.80Cr - 1.8Ni - 0.25Mo (0.35 - 0.40C) (4337)
Equivalent Sections of Certain Shapes to Round Bars
Heat Treatment, Martensitic Corrosion-Resistant Steel Parts
Heat Treatment, Precipitation-Hardening Corrosion-Resistant and Maraging Steel Parts
Heat Treatment, Austenitic Corrosion-Resistant Steel Parts
Determining Decarburization and Carburization in Finished Parts of Carbon and Low-Alloy Steels
Steel Bars, Forgings, and Rings 0.50Cr - 0.55Ni - 0.25Mo (0.33 – 0.38C) (8735)
Steel, Corrosion and Heat-Resistant, Investment Castings 19Cr - 9.5Ni (CF-3) Solution Heat Treated
Bracket, Angle, 90°, Corrosion and Heat Resistant Steel UNS S41000, .190 Bolt
Steel, Corrosion and Heat-Resistant, Investment Castings 17Cr - 13Ni - 1.9Mo Solution Heat Treated
Forgings, Magnesium Alloy, 2.0Th - 0.78Mn (HM21A - T5), Precipitation Heat Treated
NUT, SELF-LOCKING, PLATE, TWO LUG, LOW HEIGHT, UNS S66286, CLASS: 125 KSI/800 °F
Heat Treatment of Low-Alloy Steel Parts Minimum Tensile Strength 220 ksi (1517 MPa) and Higher
Automotive Ductile Iron Castings for High Temperature Applications
Steel Bars, Forgings, and Rings 0.50Cr – 0.55Ni – 0.25Mo (0.33 – 0.38C) (8735)
Aluminum Alloy, Die Forgings, 5.6zn 2.5mg 1.6cu 0.23cr Solution and Precipitation Heat Treated
Ductile (Nodular) Iron Castings, Sand 60000 psi (415 MPa) Tensile Strength Ferritize Annealed
Mechanical Properties of Heat Treated Wrought Steels
Treatment of locomotive feedwater